Methods of increase of wear resistance and resource of operation of soil pumps

Authors

  • O. Dauletbekuly
  • K. D. Baijumanov

Keywords:

Groundwater pump, hydroabrasive deterioration, wear resistance, abrasive particle, cavitation, polyurethane, electrical insulators, frequency converters, microstructure.

Abstract

Hydroabrasive wearout and cavitation of the soil pump are considered in the article. The essence and process of hydro abrasive wear. Improve the designs of pumps during their operation, and is also considered the main sources of problems. Also the analysis of ways for increase of wear resistance and energy efficiency of work during operation are made.

References

1. Povetkin V.V. – Gruntovoy nasos.- Innovatsionnyi patent RK, № 24120. – 15.06.2011.
2. Bachus L, Custodio A. – Know and Understand Centrifugal Pumps. – Elsevier, Oxford. – 2003.
3. Vinogradov V.N., Sorokin G.M., Kolokolnikov M.G. – Abrazivnoe iznashivanie. – M.: Mashinostroenie. – 1990. – P.221.
4. Suprun V.K. – Abrazivnyiy iznos gruntovyih nasosov i borba s nim. – M.: Mashinostroenie. – 1972. – P.103.
5. Tomashov N.D., Chernova G.P. – "Teoriya korrozii i korrozionnostoykie konstruktsionnyie splavyi". – iz-vo Metallurgiya. – M.: 1986. – P.234.

Downloads

Published

2015-10-19

How to Cite

Dauletbekuly, O., & Baijumanov, K. D. (2015). Methods of increase of wear resistance and resource of operation of soil pumps. International Journal of Mathematics and Physics, 6(1), 4–7. Retrieved from https://ijmph.kaznu.kz/index.php/kaznu/article/view/109